Calcium Silicate Bricks

Calcium Silicate Bricks

Calcium Silicate Bricks

CALCIUM SILICATE THERMAL INSULATION

Slab, Lags, Bricks, Pipes & Powder up to 1000 0C

Insulation brick based on Calcium Silicate is reacted Calcium Silicate containing reinforcing fibers (non-asbestos). It offers thermal efficiency of flexible insulation like mineral wool and strength of conventional Insulation Bricks.

Insulation pipes are ideal replacement for fibrous insulation and are un-matched in places where insulation is exposed to water, floor traffic, and impact loads etc.

Insulations based on Calcium Silicate meet specifications as under: –

  • IS 8154 & 8428
  • Relevant Naval Specifications
  • ASTM C 533-90
  • B.S.3958 part II.

Advantages:

  • Low Thermal Conductivity
  • Rigid & Light Weight (Density 250 kg/M3)
  • Good Mechanical Strength (Above 10kg./cm2)
  • Fire Resistant
  • Low shrinkage
  • Low specific Heat
  • Non Combustible & Non Corrosive
  • Low Maintenance Cost
  • Re-usable & Long life
  • Easily Workable (cuts easily)

Application :

Cement Preheaters / Precalciners, Coolers, TAD etc.
Aluminium Reduction pots, Other Thermal Process Equipment
Glass Furnace, Recuperations, Annealing etc.
Steel Various types of furnaces as refractory back up.
Power Plants Boilers, Steam Lines, Recuperators etc.
Fertilizers Reformers, Steam Lines, Furnaces
Petrochemicals & refineries Incinerators, High Temp. Equipments, Hot Gas & Chemical Lines etc
Ceramic Tunnel Kilns.
Ship Building Boilers, Turbines, Steam Lines, Fuel Gas ducts etc.
Chemicals Boilers, High Temp. Reactors, Fuel Gas ducts, Steam / Thermic fluid lines, Dryers, Furnaces etc.
Others Significant fuel saving can be obtained in Sugar Mills, Foundries Rolling Mills and other industries, which use thermal equipments at High temperature
Properties S 9428 ASTM C533:90 JR GRADE
Temperature © MAX. – TYPE I TYPE II 800 1000
Bulk Density: (kg/m3)

TEST VALVES

Avg. value:
950 649 871 800 1000
– – – – –
– – – – –
Compressive strength,

Reduction in thickness, max.

Dry, under a load of 415 KN/m2

Wet, under a load of 170 KN/m2

After 18 hrs. Of immersion in water.

Dry, under a load of 345 KN/m2

After 24 hrs heat soak:
– – – – –
– – – – –
5% 5% 5% 3% 3%
5% – – 3.5% 3.5%
– – – – –
5% – – 3.5% 3.5%
Content – – – –
Flexural Strength (KN/m2) min. 240 310 310 400 400
Heat resistance after heat soak at max.
Temp. For 24 hrs.

Linear shrinkage (length),

Max. :

Typical:

Loss in mass. Max:
– – – – –
– – – – –
– – – – –
2% 2% 2.5% 2% 2%
– – – 1.6% 1.8%
15% – – 15% 15%
Thermal Conductivity (W/mk)

Max. At mean temp.

200 C

300 C

400 C

500 C
– – – – –
– – – – –
0.080 0.079 0.095 0.070 0.080
0.097 0.095 0.110 0.080 0.090
0.121 – 0.136 – 0.105
0.147 – – – 0.120
Cold crushing Strength (CCS)

(Kg/cm2), min

Light Grade (k/value0.12W/mk)

Medium Grade (“ 0.15W/mk)
– – – – –
– – – – –
– – – 10 25
– – – – –